EverEdge™ 2.0 Technology

WHY DO SOME INSTRUMENTS SHOW AN INITIAL SPIKE IN SHARPNESS? An initial spike in sharpness is caused by unwanted burr formation on the cutting edge. A burr is a small piece of metal that is attached to the blade. Burr formations occur when a finishing step is done too quickly or not at all—an indication of poor process control. EverEdge™ 2.0 Scalers do not have burr formations due to our refined process—allowing them to start out sharp and stay sharper longer. The Science of EverEdge ™ 2.0 How EverEdge ™ 2.0 Technology Compares Against Competitors

Edge Retention Through 500 Strokes 2

(Through test media 2 )