Chiselling out, exposing, rust removal
1
2
3
Cleaning the steel reinforcement by dry blasting with solid blasting media. Degree of rust removal, Sa 2½ to DIN EN 12944-4
Typical decay of inadequately protected concrete
Exposing corroded steel reinforcement
Concrete repair – simple and reliable
Specifically, carrying out concrete repairs straightforwardly, quickly and reliably means using only one product. The material provides corrosion protection, good adhesion means that a bonding bridge is not required and the elevated fines content means that the surface can be smoothed in a similar way to a filler. Areas of application are conven- tional building construction and also light-weight concrete objects. KEIM Concretal- Universalmörtel-S – one product for every job.
One product for every job
4
5
Fill defects with mineral KEIM Concretal-Universalmörtel in the prewetted substrate, use without specific corrosion protection and bonding bridge. Layer thicknesses of 0.5–5 cm are possible, multiple layers must be used from a thickness of approx. 2.5 cm. KEIM Concretal- Universalmörtel-S can be directly smoothed.
Apply two protective coats of KEIM Concretal-W a) diluted priming coat b) undiluted finishing coat in each case applied by brush, roller or airless sprayer