Buildings 2025 , 15 , 1702

9of 14

OSB-1 sample showed no significant statistical differences compared to either the OSB-C or OSB-2 samples. These results were similar to those obtained by Núñez-Decap et al. [14], who compared formaldehyde-based and protein-based wood adhesives, in tensile strength tests, which were also statistically comparable.

( a )

( b )

Figure 4. Load–displacement curves of each sample subjected to bending test in ( a ) flatwise and ( b ) edgewise positions.

Figure5. Modes of failure of each sample result after the bending test.