4. If more than 48 hours is left between coats then it is ESSENTIAL to abrade to remove surface hardness. Leave overnight to condition before proceeding

760D

Decking

1. First coat: Apply liberally in direction of grain, avoid puddles. Leave to dry 2. Subsequent coats: As required to satisfy surface porosity. 3. Pay special attention to freshly sawn ends of decking boards and ensure treatment with a suitable preservative before applying finishing system

760E

Existing decking treated

1. NOTE: Sadolin Decking Oil is only suitable for use on bare or previously oiled decking 2. First coat: Apply liberally in direction of grain, avoid puddles. Leave to dry 3. Subsequent coats: As required to satisfy surface porosity. 4. Pay special attention to freshly sawn ends of decking boards and ensure treatment with a suitable preservative before applying Sadolin Decking Oil

770 External doors

1. Bottom edges: Prime and coat before hanging doors.

780 Bead glazing to coated wood

1. Before glazing: Apply first two coats to rebates and beads.

780A

Bead glazing- new wood

1. Before glazing: Apply full system to rebates and beads.

790 Linseed oil putty glazing

1. Setting: Allow putty to set for seven days. 2. Sealing 2.1. Within a further 14 days, seal with a solvent-borne primer. 2.2. Fully protect putty with coating system as soon as it is sufficiently hard. 2.3. Extend finishing coats on to glass up to sight line.

790A

Glazing sealant

1. Putty glazing is NOT recommended with Sadolin woodcare systems 2. Glaze using a sealant in accordance with Section 4.2 of Glazing Federation manual. 2.1. Refer to BS 8000-7: 1990 and BS 6262.

Ω E nd of Section