Achteck katalog 2025

Milling Milling Cutters

Compatible Inserts

● Good Conditions Bad Conditions

General Conditions

Machining conditions

● ● ● ● ●

Dimension (mm)

P

M K N H

Insert shape

Product code

L W1 S REBSD1AN

APKT 1705PER-DT

16.510.765.630.8 2.2 4.4 11°

● ●

● ●

APKT 170516R-DT

16.810.745.631.6 1.7 4.4 11°

●: Standard stock ○: Made-to-Order

Materials

Cutting depth and feed

AP..1705..

Geometry DT fz

ap

Hardness (HB)

Tensile strength (N/mm 2 )

ISO

Material classification

(mm)

min

max

min

max

<600 <950

<180 <280

Unalloyed steel

0.08

0.25

700-950 950-1200 1200-1400

200-280 280-355 355-415

Alloyed steel

0.06

0.22

Duplex stainless steel Austenitic stainless steel

778 675

230 200 300 220 260 250

0.06

0.20

Precipitation-hardening stainless steel

1013

Grey cast iron

700 880 800 260 447 943

Nodular cast iron Malleable cast iron

0.50

15.50

0.08

0.25

Aluminum

75

-

-

Aluminum alloy Fe-based alloy Co-based alloy Ni-based alloy

130 280 320 350 370

1076 1177 1262

0.06

0.18

Ti-alloy

Hardened steel Chilled cast iron

- -

50-60HRC

-

-

55HRC *The recommended cutting conditions always refer to general conditions. These cutting conditions should be adjusted according to the practical machine rigidity, tools, workpiece clamping and coolant. Average chip thickness (hm)=fz x sinkr.