Achteck katalog 2025

Milling Milling Cutters

Spare parts

Cutter diameter (mm)

Screw

Wrench

Torque

∅ 25-50

3.0Nm

SP035086

DT-TP10

Compatible Inserts

● Good Conditions Bad Conditions

General Conditions

Machining conditions

● ● ● ●

Dimension (mm)

P

M K S H

Insert shape

Product code

IC S REBSD1AN

XDLT 090408ER-MM3

9.525 4.76 0.8 1.3 3.9 15°

● ●

XDMW 090408ER-HR2

9.506 4.76 0.8 1.6 3.9 15°

●: Standard stoc k ○ : Made-to-Order

Materials

Cutting depth and feed

XD..0904..

High feed milling

Plunging

Hardness (HB)

Tensile strength (N/mm 2 )

ISO

Material classification

ap

fz

ae

fz

(mm) min max min max min max min max

<600 <950

<180 <280

Unalloyed steel

0.30 1.50

0.05 0.15

700-950 950-1200 1200-1400

200-280 280-355 355-415

Alloyed steel

0.30 1.50

0.05 0.12

Duplex stainless steel Austenitic stainless steel

778 675

230 200 300 220 260 250

0.20 0.80

0.05 0.10

Precipitation-hardening stainless steel

1013

Grey cast iron

700 880 800 260 447 943

Nodular cast iron Malleable cast iron

0.30 1.50

0.05 0.15

0.20 1.20

0.00 7.00

Aluminum

75

− −

− −

Aluminum alloy Fe-based alloy Co-based alloy Ni-based alloy

130 280 320 350 370

1076 1177 1262

0.10 0.50

0.05 0.10

Ti-alloy

Hardened steel Chilled cast iron

- -

50-60HRC

0.30 1.00

0.05 0.10

55HRC *The recommended cutting conditions always refer to general conditions. These cutting conditions should be adjusted according to the practical machine rigidity, tools, workpiece clamping and coolant. Average chip thickness (hm)=fz x sinkr.

359