Milling Milling Cutters
Compatible Inserts
● Good Conditions Bad Conditions
General Conditions
Machining conditions
●
● ● ● ●
Dimension (mm)
P
M K N S
Insert shape
Product code
IC S REBSD1AN
SDMT 09T308N-MM4
9.525 3.97 0.8
- 3.9 15°
●
● ● ● ●
SDMT 09T320N-MM4
9.520 3.97 2.0
- 3.9 15°
●
● ● ● ● ●
SDMT 09T308N-MR2
9.525 3.97 0.8
- 3.9 15°
●
● ● ● ●
SDMT 09T320N-MR2
9.520 3.97 2.0
- 3.9 15°
●
● ● ● ●
●: Standard stoc k ○ : Made-to-Order
Materials
Cutting depth and feed
SD..09T3..N..
Geometry
ap
MM4
MR2
Hardness (HB)
Tensile strength (N/mm 2 )
ISO
Material classification
fz
(mm)
min
max
min max min max
<600 <950
<180 <280
Unalloyed steel
0.05
0.25
0.05
0.35
700-950 950-1200 1200-1400
200-280 280-355 355-415
Alloyed steel
0.05
0.22
0.05
0.30
Duplex stainless steel Austenitic stainless steel
778 675
230 200 300 220 260 250
-
-
0.08
0.35
Precipitation-hardening stainless steel
1013
Grey cast iron
700 880 800 260 447 943
Nodular cast iron Malleable cast iron
0.10
5.50
0.08
0.30
0.08
0.30
Aluminum
75
-
-
-
-
Aluminum alloy Fe-based alloy Co-based alloy Ni-based alloy
130 280 320 350 370
1076 1177 1262
0.05
0.30
-
-
Ti-alloy
Hardened steel Chilled cast iron
- -
50-60HRC
-
-
-
-
55HRC *The recommended cutting conditions always refer to general conditions. These cutting conditions should be adjusted according to the practical machine rigidity, tools, workpiece clamping and coolant. Average chip thickness (hm)=fz x sinkr.
387
Made with FlippingBook - Online Brochure Maker