Achteck katalog 2025

Milling Solid Carbide End Mills

Solid Carbide End Mill M170 Cutting Data Recommendation

M170-4ES M170-4RS M170-6ES

Square shoulder milling (Finsih milling)

1.0D

Materials

0.02D

fz [mm/Tooth] Mill diameter [mm]

Cutting speed Vc(m/min)

ISO

Workpiece Materials

4

6

8

10

12

16

C ≤ 0.25%

Annealed 125 428

0.25 < C ≤ 0.55%

Annealed 190 639

0.25 < C ≤ 0.55%

Heat-treated 210 708

Unalloyed steel

Annealed 190 639

C > 0.55%

Heat-treated 300 1013

200-300

0.080

0.126

0.170

0.216

0.237

0.266

C > 0.55%

Free cutting steel

Annealed 220 745

Annealed

175 591

Heat-treated

300 1013

200-300

0.080

0.126

0.170

0.216

0.237

0.266

Low-alloyed steel

Heat-treated

380 1282

180-260

0.076

0.120

0.162

0.206

0.226

0.254

Heat-treated

430 1477

170-260

0.073

0.115

0.155

0.197

0.216

0.242

Annealed

200 675

High-alloyed steel and highalloyed tool steel

Hardened and tempered

300 1013

200-300

0.080

0.126

0.170

0.216

0.237

0.266

Hardened and tempered

400 1361

180-260

0.076

0.120

0.162

0.206

0.226

0.254

Ferritic/Martensite,Annealed

200 675

Stainless steels

Martensite,Heat-treated

330 1114

Austenitic,hardened

200 675

Stainless steels

Austenitic,precipitation hardened stainless steel(PH stainless steel)

300 1013

Austenitic,ferritic,duplex

230 778

Ferritic

200 400

230-340

0.090

0.140

0.190

0.240

0.164

0.296

Malleable cast iron

Pearlitic

260 700

220-310

0.077

0.119

0.162

0.204

0.139

0.252

Low tensile strength

180 200

230-340

0.090

0.140

0.190

0.240

0.164

0.296

Grey cast iron

High tensile strength/Austenitic

245 350

230-320

0.081

0.126

0.171

0.216

0.148

0.266

Ferritic

155 400

230-340

0.090

0.140

0.190

0.240

0.164

0.296

Nodular cast iron

Pearlitic

265 700

220-310

0.077

0.119

0.162

0.204

0.139

0.252

GGV(CGI) Wrought aluminum alloy Cast aluminum alloy

230 400

210-310

0.072

0.112

0.152

0.192

0.131

0.237

Non-aging alloy

30

-

Aged alloy

100 340

≤ 12% Si, non-aging alloy

75

260

≤ 12% Si, aged alloy

90

310

> 12% Si, non-aging alloy

130 450

Magnesium alloy

70

250

Unalloyed,electrolytic copper

100 340

Copper and copper alloy(bronze/ brass)

Brass,bronze,red brass

90

310

Cu alloy,short chip

110 380

High tensile,Ampco alloy

300 1010

Annealed 200 680 Aged 280 940 Annealed 250 840 Aged 350 1180 Cast 320 1080

Fe-based

Fe-based alloy

Ni or Co based

Pure Titanium

200 680

Titanium alloy

α and β alloy, aged

375 1260

β alloy

410 1400

Tungsten alloy

300 1010

Molybdenum alloy

300 1010

Hardened and tempered

50HRC -

190-280

0.045

0.070

0.095

0.120

0.132

0.148

Hardened steel

Hardened and tempered

55HRC -

110-160

0.032

0.049

0.067

0.084

0.092

0.104

Hardened and tempered

60HRC -

80-140

0.027

0.042

0.057

0.072

0.079

0.089

Chilledcastiron Hardened and tempered

55HRC -

170-260

0.041

0.063

0.086

0.108

0.119

0.133

The cutting data are average recommended values. For special applications, adjustment is needed.