Step 4: Place 10 sheets of normal copy paper on the rubber of your press, followed with your Teflon sheet on top. Place the silver side (glue side) of the video flex facing the Teflon sheet.

Step 5: Place the sublimation print ontop. The print facing the white side of the video flex. Secure with heat tape to the Teflon. Press with medium to high pressure 165°C and 90 seconds.

When done, remove the print and let the video flex cool down completely, before you remove it from the Teflon sheet.

Step 6: Set your press to 120°C and 15 seconds. Let the press cool down to this temperature. Cut the 10 sheets of copy paper the same length as your printed video flex and place it underneath your Teflon sheet on the edge of the press. You will press on the edge because you don ’ t want the entire shield to be exposed to heat. This is very important.