Step 7: Place your sublimated sheet video flex on top of the shield and line it up. Very important : You need to rub out all bubbles with your fingers or soft cloth so that it is smooth and in line before you press it.
Step 8: Place the shield on the edge of your press, make sure the bottom of your print is in line with the bottom of your press edge and secure it with heat tape to the Teflon sheet. The heat tape should not be on your print but the sides of the shield.
Step 9: Cover the sides of the shield that are exposed to the element of your press with 5 sheets of copy paper and put a silicone sheet on top of your print. Press for 15 seconds on 120°C. While you press it, hold the piece of the mask that is sticking out of the press with your hands in line with the press. The reason for this is, the heat will soften the shield and it will bend. So keep it up for now until it is cooled down.