Turning

Grade Application Guide

Turning grade application

Materials

PVD coated

CVD coated Uncoated

Material classification

Tensile strength ( N/mm 2 )

Hardness (HB)

ISO

AP301U

AP330M AC230P AW100K

● ● ● ● ● ● ● ● ◐ ◐ ◐

● ● ● ● ● ● ● ●

● ● ● ● ●

<600

<180

-

Unalloyed steel

<950

<280

-

700-950

200-280

-

P

Alloyed steel

950-1200

280-355

-

1200-1400

355-415

-

Duplex stainless steel

778

230

-

-

Austenitic stainless steel

675

200

-

-

M

Precipitation-hardening stainless steel

1013

300

-

-

● ● ●

Grey cast iron

700

220

-

-

K

Nodular cast iron

880

260

-

-

Malleable cast iron

800

250

-

-

● ●

Aluminum

260

75

-

-

-

N

Aluminum alloy

447

130

-

-

-

Fe-based alloy

943

280

-

-

-

-

Co-based alloy

1076

320

-

-

-

-

S

Ni-based alloy

1177

350

-

-

-

-

Ti-alloy

1262

370

-

-

-

-

Hardened steel

-

50-60HRC

-

-

-

-

H

Chilled cast iron

-

55HRC

-

-

-

-

● 1st choice ◐ 2nd choice -

Inapplicable