Milling

Dimension (mm)

P

M

K

S

Product code

IC

S

● ●

● ●

ROHT 1605M8E-MM3

16

5.56

ROMT 1605M6E-MR6

16

5.56

●: Stock available ▲: Stock available now but will be replaced in the future.

Materials

Cutting depth and feed

RO..1605..

MM3

MR6

ap fz 0.1 < ap ≤ 1.5 1.5 < ap ≤ 8 0.1 < ap ≤ 1.5 1.5 < ap ≤ 8 (mm) min max min max min max min max min max

Material classification

Tensile strength (N/mm 2 )

Hardness (HB)

ISO

<600 <950

<180 <280

Unalloyed steel

0.20 0.65 0.12 0.35 0.20 0.68 0.12 0.38

P

700-950

200-280 280-355 355-415

Alloyed steel

950-1200

0.18 0.60 0.10 0.32 0.18 0.65 0.10 0.35

1200-1400

Duplex stainless steel

778 675

230 200 300 220 260 250

M

Austenitic stainless steel

0.15 0.55 0.10 0.30 0.15 0.58 0.10 0.32

Precipitation-hardening stainless steel

1013

Grey cast iron

700 880 800 260 447 943

K

0.80 8.00

Nodular cast iron

-

-

-

-

-

-

-

-

Malleable cast iron

Aluminum

75

N

-

-

-

-

-

-

-

-

Aluminum alloy Fe-based alloy Co-based alloy

130 280 320 350 370

1076 1177 1262

S

0.15 0.50 0.10 0.30

-

-

-

-

Ni-based alloy

Ti-alloy

Hardened steel Chilled cast iron

- -

50-60HRC

H

-

-

-

-

-

-

-

-

55HRC *The recommended cutting conditions always refer to general conditions. These cutting conditions should be adjusted according to the practical machine rigidity, tools, workpiece clamping and coolant. Average chip thickness (hm)=fz x sinkr.