Milling
Solid Carbide End Mill Eco Line Cutting Parameters
M145-2ES M145-3ES M145-3EL Cutting speed Vc(m/min)
2.5D
Square shoulder milling
Materials
0.15D
Tensile strength Rm(N/ mm²)
fz [mm/Tooth] Mill diameter [mm]
Brinell hardness (HB)
Material classification
ISO
2 4
6 8
10 12 14
16
20
C ≤ 0.25%
Annealed 125
428
0.25 < C ≤ 0.55%
Annealed 190
639
0.25 < C ≤ 0.55%
Heat-treated 210
708
Unalloyed steel
Annealed 190
639
C > 0.55%
Heat-treated 300
1013
C > 0.55%
Free cutting steel (short-chip) Annealed 220
745
Annealed
175
591
P
Heat-treated
300
1013
Low-alloyed steel
Heat-treated
380
1282
Heat-treated
430
1477
Annealed
200
675
High-alloyed steel and high-alloyed tool steel
Hardened and tempered
300
1013
Hardened and tempered
400
1361
Ferritic/martensitic, annealed
200
675
Stainless steel
Martensitic, heat-treated
330
1114
Austenitic, quench hardened
200
675
M
Stainless steel
Austenitic, precipitation hardened (PH)
300
1013
Austenitic/ferritic, duplex
230
778
Ferritic
200
400
Malleable cast iron
Pearlitic
260
700
Low tensile strength
180
200
Grey cast iron
K
High tensile strength/austenitic
245
350
Ferritic
155
400
Nodular cast iron
Pearlitic
265
700
GGV(CGI)
230
400
Non-aging
30
-
150~200 0.025 0.040 0.055 0.065 0.090 0.110 0.120 0.140 0.160
Wrought aluminium alloys
Aged
100
340 120~150 0.025 0.040 0.055 0.065 0.090 0.110 0.120 0.140 0.160
≤ 12% Si, non-aging
75
260
150~200 0.025 0.040 0.055 0.065 0.090 0.110 0.120 0.140 0.160
Cast aluminium alloys
≤ 12% Si, aged
90
310 120~150 0.025 0.040 0.055 0.065 0.090 0.110 0.120 0.140 0.160
> 12% Si, non-aging
130
450 120~150 0.025 0.040 0.055 0.065 0.090 0.110 0.120 0.140 0.160
N
Magnesium alloys
70
250 150~170 0.025 0.040 0.055 0.065 0.090 0.110 0.120 0.140 0.160
Unalloyed, electrolytic copper
100
340 120~150 0.025 0.040 0.055 0.065 0.090 0.110 0.120 0.140 0.160
Brass, bronze, red brass
90
310 120~150 0.025 0.040 0.055 0.065 0.090 0.110 0.120 0.140 0.160
Copper and copper alloys
Cu alloys, short-chipping
110
380
120~150 0.025 0.040 0.055 0.065 0.090 0.110 0.120 0.140 0.160
High-tensile, Ampco alloy
300
1010
Annealed 200
680
Fe-based
Hardened
280
940
Heat-resistant alloys
Annealed 250
840
Ni or Co based
Hardened 350
1180
Cast
320
1080
S
Pure titanium
200
680
Titanium alloys
α and β alloys, hardened
375
1260
β alloys
410
1400
Tungsten alloys
300
1010
Molybdenum alloys
300
1010
Hardened and tempered
50HRC
-
Hardened steel
Hardened and tempered
55HRC
-
H
Hardened and tempered
60HRC
-
Chilled cast iron Hardened and tempered
50HRC
-
The cutting data are average recommended values. For special applications, adjustment is needed.