Achteck - obecný katalog

Hole machining

Recommended Cutting Speed for Materials(Dia ≥63.50mm)

Grade

Feed fn mm/r

Brinell hardness (HB)

Cutting speed Vc m/min

Workpiece material

Insert

Drilling dia mm

P

I

C

≥63.50 0.18-0.35 0.18-0.35 0.18-0.35 0.18-0.35 0.18-0.35 0.16-0.35 0.18-0.30 0.18-0.30 0.16-0.30 0.16-0.30 0.15-0.30 0.15-0.30 0.16-0.35 0.16-0.35

C=0.05-0.10% C=0.10-0.25% C=0.25-0.55% C=0.55-0.80%

125 125 150 170 210 180 275 350 200 325 180 200 200 200 300 230 200 260 180 245 160 250 230

80-100 80-100 80-100 80-100 70-100 60-100 70-100 70-100 60-100 60-100 50-100 50-100

Unalloyed steel

AP301U(N)

High carbon steel

Carbon tool steel Non-Hardened

AP301U(N)

P

Low-alloyed steel

Tempered Tempered Annealed

AP301U(N)

High-alloyed steel

AP301U(N)

Hardened tool steel Non-alloyed steel Low-alloy ( alloy<5%)

Cast steel

AP301U(N)

Non-Hardened/Ferritic/martensitic

50-90 50-90

Austenitic

M

Stainless steel

AP301U(N)

Austenitic, precipitation hardened (PH)

Austenitic/ferritic, duplex

Ferritic Pearlitic

Malleable cast iron

AP301U(N)

Low tensile strength High tensile strength

Grey cast iron

AP301U(N)

K

Ferritic Pearlitic

Nodular cast iron

AP301U(N)

GGV (CGI)

non-aging

30

65-130 65-130 65-130 65-130 65-130 65-130 65-130 65-130 65-130

0.10-0.30 0.10-0.30 0.10-0.30 0.10-0.30 0.10-0.30 0.10-0.30 0.10-0.30 0.10-0.30 0.10-0.30 0.15-0.30 0.15-0.30 0.15-0.30 0.15-0.30 0.15-0.30 0.15-0.30 0.15-0.30 0.15-0.30

Wrought aluminium alloys

AP301U(N)

aged

100

≤ 12% Si, non-aging

75 90

Cast aluminium alloys

≤ 12% Si, aged

AP301U(N)

> 12% Si, non-aging

130

N

Magnesium alloy

70

Unalloyed, electrolytic copper Brass, bronze, red brass Cu alloys, short-chip High tensile, Ampco alloy

100

AP301U(N)

90

Copper and copper alloys (bronze/brass)

110 300 200 280 250 350 320 200 375 375 410

AP301U(N)

Fe-based annealed Fe-based hardened

20-65 20-65 20-65 20-65

Ni or Co-based annealed Ni or Co-based hardened

Heat-resistant alloys

AP301U(N)

Ni or Co-based cast

S

Pure titanium

30-100 30-100 30-100 30-100

α alloys

Titanium alloys

AP301U(N)

α and β alloys

β alloys

Hardened steel Chilled cast iron

Hardened and tempered

43-47 HRC 47-60 HRC

H

*) Insert position-P , I , C P=peripheral insert , I=intermediate insert, C=center insert