Selenis General Presentation - USA

Polyester modification Acid side

PET HomoPolymer

Acid – Side Modification

COOH

COOH

O

O

O

O

[ CH 2 CH 2 O C

[ m

[ CH 2 CH 2 O C

C [ n

COOH

C-O

COOH terephthalic acid

isophthalic acid

EG

TPA

EG

TPA

IPA versus TPA

Adding IPA while reducing TPA

Applications PET Homopolymer as used in many BOPET applications PET Bottle-grade PET grades for heavy gauge sheet extrusion up to 5mm PET sealing layer on CPET trays BOPET coextrusion

% of modification 0% of modification approx. 2% IPA

5 to 10% IPA 5 to 10% IPA > 15% up to 36%