Navy Spec Welding Audits – Common Areas of Findings

welding heat control

Common Audit Finding

Requirement

Correction

Welder not checking preheat and interpass min/max at appropriate times or locations

Ensure welders check preheat and interpass temperatures at specified times and locations.

S9074-AR-GIB-010/278 4.2.2

Calibrate devices used for checking temperatures and ensure their accuracy.

Device for checking minimum and maximum preheat and Interpass

S9074-AR-GIB-010/278 4.2.2, S9074-AQ-GIB-010/248 4-7.2.c

temperatures not accurate (infrared device not calibrated, canted contact pyrometer)

Post weld heat treatment (see Tech Pub 278 Section 8 if applicable or for guidance): Non- weld spec driven thermal processes (such as stress relief of formed of CuNi fittings or nitriding) effectively become PWHT that must be qualified

Qualify non-weld spec driven thermal processes as PWHT if applicable.

S9074-AQ-GIB-010/248 4-7.2.c

Oven temperature measurement devices not calibrated

Regularly calibrate oven temperature measurement devices.

S9074-AQ-GIB-010/248 4-7.2.c