NOTE:

Steps 3 to 6 below will depend on the OEM’s requirements. Consult the OEM -specific instructions. If the OEM demands both gelcoat and paint, proceed with steps 3 to 6. If the OEM only requires paint, omit steps 3 to 5..

3. Calculate and then weigh out and mix the required amount of gelcoat, and apply this to the filler, distributing it evenly and to the specified layer thickness with a plastic scraper. Verify the layer thickness using a wet film gauge.

4. Allow the gelcoat to fully cure in accordance with the TDS.

5. Sand the gelcoat to the required surface finish in accordance with the TDS for the paint.

6. Calculate and then weigh out and mix the required amount of paint and apply this to the sanded gelcoat, distributing it evenly and to the specified layer thickness using a foam roller. Verify the layer thickness with a wet film gauge.