SPEEDS AND FEEDS FOR TURNING Machinery's Handbook, 31st Edition
1105
Tool Life
Cutting Speed
15 min 45 min 90 min 180 min
V 15 = 3466 fpm
V 45 = V 15 3 0.80 = 2773 fpm V 90 = V 15 3 0.70 = 2426 fpm
V 180 = V 15 3 0.61 = 2114 fpm Depth of cut, feed, and lead angle remain the same as in Example 3. Notice, increasing the tool life from 15 to 180 minutes, a factor of 12, reduces the cutting speed by only about one-third of the V 15 speed. Table 6. Cutting Speeds and Feeds for Turning Copper Alloys Group 1 Architectural bronze (C38500); Extra-high-headed brass (C35600); Forging brass (C37700); Free-cutting phosphor bronze, B2 (C54400); Free-cutting brass (C36000); Free-cutting Muntz metal (C37000); High-leaded brass (C33200; C34200); High-leaded brass tube (C35300); Leaded commercial bronze (C31400); Leaded naval brass (C48500); Medium-leaded brass (C34000) Group 2 Aluminum brass, arsenical (C68700); Cartridge brass, 70% (C26000); High-silicon bronze, B (C65500); Admiralty brass (inhibited) (C44300, C44500); Jewelry bronze, 87.5% (C22600); Leaded Muntz metal (C36500, C36800); Leaded nickel silver (C79600); Low brass, 80% (C24000); Low-leaded brass (C33500); Low-silicon bronze, B (C65100); Manganese bronze, A (C67500); Muntz metal, 60% (C28000); Nickel silver, 55-18 (C77000); Red brass, 85% (C23000); Yellow brass (C26800) Group 3 Aluminum bronze, D (C61400); Beryllium copper (C17000, C17200, C17500); Commercialbronze, 90% (C22000); Copper nickel, 10% (C70600); Copper nickel, 30% (C71500); Electrolytic tough pitch copper (C11000); Guilding, 95% (C21000); Nickel silver, 65-10 (C74500); Nickel silver, 65-12 (C75700); Nickel silver, 65-15 (C75400); Nickel silver, 65-18 (C75200); Oxygen-free copper (C10200) ; Phosphor bronze, 1.25% (C50200); Phosphor bronze, 10% D (C52400) Phosphor bronze, 5% A (C51000); Phosphor bronze, 8% C (C52100); Phosphorus deoxidized copper (C12200)
Uncoated Carbide
Polycrystalline Diamond
HSS
f = feed (0.001 in/rev), s = speed (ft/min) Metric Units: f 3 25.4 = mm/rev, s 3 0.3048 = m/min Opt. Avg. Opt.
Wrought Alloys Description and UNS Alloy Numbers
Material Condition
Speed (fpm)
Avg.
f s f s f s
A CD A CD A CD
300 350 200 250 100 110
28 1170
13 1680
Group 1
28 715 28 440
13 900 13 610
Group 2
7 1780
13 2080
Group 3
Abbreviations designate: A, annealed; CD, cold drawn. The combined feed/speed data in this table are based on tool grades (identified in Table 16) as follows: uncoated carbide, 15; diamond, 9. See the footnote to Table 7.