Univet Cleanroom Catalogue - ENGLISH

VALIDATED TECHNOLOGY 611 POLYCARBONATE Lens

128 g

autoclave sterilization

Sterilization with STEAM 121°C for 30min in 1 ATM

REFERENCE PARAMETERS Lens Δl = 73.3% VLT= visible light trasmittance Δl = elongation% VLT = 85.8% Elastic Band

LIFE CYCLE

number of cycles 0 5 10 15 20 25 30 35 40 45

suggested action

suggested action Replace the goggles

Change the lens

Mask elements

Number of cycles

0÷20

20÷30

30÷40

Frame

No alteration

No alteration

No alteration

Lens

VLT = 82.6% Δl = 63.3% No alteration

VLT = 82.3% Δl = 61.2% No alteration

VLT = 81.4% Δl = 58.3% No alteration

Elastic band

Buckle

Resistance to fogging of oculars EN166:2001 Clause 7.3.2

SAMPLE

TIME TO FOGGING [s]

‘N’ MARKING REQUIREMENT [s]

AF121

>30

>8

Resistance to surface damage by fine particles EN166:2001 Clause 7.3.1

SAMPLE REDUCED LUMINANCE FACTOR [cd/lx·m 2 ]

‘K’ MARKING REQUIREMENT [cd/lx·m 2 ]

AF121

1.2

<5

611

Lens

128 g

β and γ ray sterilization

Reference

1 cycle

5 cycles

10 cycles

15 cycles

20 cycles

Visible light trasmittance (VLT) Lens

89.1%

88.9%

88.7%

89.1%

88.5%

88.3%

Variation

-0.2%

-0.4%

-0.4%

-0.6%

-0.8%

87.2%

85.6%

78.2%

73.1%

66.4%

63.6%

Visible light trasmittance (VLT) POLYCARBONATE Lens

Variation

-1.8%

-10%

-16%

-24%

-27%

REF 5 cycles 10 cycles 15 cycles 20 cycles