PAPERmaking! Vol12 Nr2 2026

Coatings 2026 , 16 , 299

9of 25

Table 3. List of selected roughness parameters that were obtained from analysis of surface profiler images.

Symbol

Name

Description

Average roughness over a measurement area

Arithmetic mean of the absolute values of the surface departures from the mean plane. This parameter is derived from bearing analyses and ex- presses the volume (e.g., of a fluid filling the core sur- face) that the surface would sup- port from 10% to 80% of the bearing area ratio. This parameter is derived from bearing analyses and expresses the volume (e.g., of a fluid filling the valleys) that the surface would support from 80% to 100% of the bearing area ratio.

Sa

Sc

Core void volume

Sv

Surface void volume

Two of the parameters in Table 3 are derived from bearing analyses. Bearing analyses are commonly utilised in tribology and can also be applied to other fields. The details of bearing analysis curves are explained elsewhere [76]. The total surface volume ( V s )was defined according to the following:

V s = Sc + Sv

(1)

To distinguish between surface roughness and waviness, zero-order Gaussian regres- sion filtering (Vision 64 software program, Bruker Nano Inc., Tucson, AZ, USA) was used for the elimination of large-scale lateral components. A wavelength cutoff of 1 mm was used, as surface roughness typically scales between 0.001 mm and 1 mm [77]. Values of Sa before and after Gaussian regression filtering are shown, while Sc and Sv were calculated without filtering. All measurements of surface structure, including the Bendtsen test, were completed within 22 months after the coating trials. Grease Resistance Grease resistance was evaluated using the Kit test according to TAPPI 559 in five replicates. In this test, 12 different mixtures of castor oil, toluene and heptane are prepared—referred to as Kit solutions—which vary in surface tension and viscosity and are numbered from 1 to 12. A higher Kit number indicates a greater tendency for the solution to penetrate the specimen. A drop of each Kit solution was applied to the coated surface, and the Kit rating was defined as the highest-numbered Kit solution that did not penetrate within 15 s. This means that a high Kit rating number indicates high grease resistance. The maximum Kit rating number is 12. All grease resistance measurements were conducted two months after the coating trials. Oxygen Transmission The oxygen transmission rate (OTR) was determined in accordance with ASTM D 3985- 05 using a Mocon Ox-Tran oxygen transmission rate tester, Model 2/21 MH from Mocon, Inc., Minneapolis, MN, USA. The test area was 5 cm 2 , and the OTR measurements were carried out using air as the permeant (oxygen concentration 20.9% (by vol.) and 50% RH) in two and four replicates for Series A and the reference thick double coating, respectively. All OTR measurements were completed within three months of the coating trials. The ambient oxygen ingress rate (AOIR) was determined using air as the permeant to characterise the dynamics of oxygen permeation. The sample cells were connected to a gas permeation analyser (PermMate, Systech, IL, USA). The cell volume ( V cell )was

https://doi.org/10.3390/coatings16030299

Made with FlippingBook Online newsletter maker